Home / Hardware y Moviles / A circuit board is drawn with ultraviolet light and carved with acid

A circuit board is drawn with ultraviolet light and carved with acid

Almost nobody looks at the board everything else is mounted on. It is green, or black, covered in tiny white lettering, and it disappears under the case the moment the phone is closed. Yet a good part of a handset’s engineering lives there: a sheet of fibreglass and resin with up to fourteen layers of copper talking to each other through holes one tenth of a millimetre wide. Building it is not printing a drawing. It is photography, chemistry, drilling and pressing under pressure at two hundred degrees.

You start with a sheet that conducts nothing at all

The raw material is FR-4 laminate: glass-fibre cloth impregnated with epoxy resin and only half cured, in what the industry calls the B stage. At that point the resin can still melt and harden again, and that property is what will bond layers later on. The maker ships it as a core, with copper bonded on both faces: usually 18 micrometres for half an ounce, 35 for a full ounce. On the inner layers of a phone the copper drops to 9 or 12 micrometres, because no current flows there, only signal.

The rest of the kit is prepreg (the same cloth with B-stage resin but no copper, which will act as glue) and bare copper foil. Those three pieces build any stack-up, from the simplest two-sided board to the fourteen-layer sandwich in a flagship.

The pattern is drawn with light, not ink

Here comes the part almost nobody pictures: the circuit is not printed, it is developed. A photopolymer film, the dry film, 25 to 40 micrometres thick, is hot-rolled onto the copper. On top goes a photomask, a transparent film carrying the track pattern in black, and the whole thing is exposed to ultraviolet light. Where the light passes, the polymer cross-links and becomes insoluble; where it does not, it stays soluble.

A bath of one per cent sodium carbonate washes away the soft part and leaves the copper bare exactly where it has to go. Then the acid steps in: cupric chloride at 45 to 50 degrees dissolves the exposed copper at 20 to 40 micrometres a minute. The attack is not perfect; it also eats sideways under the polymer, and that undercut is what sets the minimum trace width: on a cheap board, 100 micrometres of track and 100 of gap; on a phone with fine lines, 40 and 40. To go below that you stop subtracting material and start adding it: the semi-additive process (mSAP) begins with a thin copper seed and grows the trace by electroplating, which allows 30 micrometres.

Finally the photopolymer is stripped with sodium hydroxide and the definitive copper is left, still covered by the layers above.

Fourteen layers baked in a press

The etched cores are stacked alternately with prepreg and loaded into a vacuum press. There the resin flows again, fills the gaps between tracks, pushes the air out and cures: about 200 degrees and 20 to 30 bar for two hours. The result is a monolithic block, and this is where one of the nastiest details lives: resin shrinks as it cures, and every layer shifts a fraction of a micrometre against the one below. Manufacturers compensate by scaling the original artwork by 0.02 or 0.05 per cent, and they check alignment against fiducial marks read by X-ray.

The laminate’s glass transition temperature, Tg, sets the ceiling: above 150 or 170 degrees the resin turns from rigid to rubbery and expands. That is why modern stack-ups use high-Tg resins and ceramic fillers, and why a phone that runs too hot ends up with faults that have nothing to do with the chip.

The holes that tie one layer to the next

A multilayer board is useless if the layers do not talk. Through-holes are drilled with tungsten-carbide bits 0.2 to 0.3 millimetres across spinning at more than 150,000 rpm; such a bit wears out after two or three thousand holes and has to be changed. Then the resin smear left by the drill is cleaned off, a copper seed layer is deposited chemically and copper is electroplated until the hole wall carries 20 or 25 micrometres. The depth-to-diameter ratio, the aspect ratio, must stay under 10 to 1 or the bath never reaches the bottom.

In a phone almost everything is a microvia 50 to 100 micrometres wide, drilled with a CO2 laser, crossing a single layer and then filled and planarised so more can be laminated on top. That is what enables HDI, high-density interconnect: several generations of staggered microvias, or outright any-layer, with free connection between adjacent layers.

The green mask and the finish nobody sees

Solder mask goes over the copper, a photoimageable ink that is exposed and developed like the dry film and then cured. It is not decoration: it insulates, prevents solder bridges and keeps moisture out. The silkscreen lettering goes on top.

Last comes the finish on the areas to be soldered, and real engineering decisions live here. HASL, dipping the board in molten tin and blowing off the excess, is cheap but leaves uneven surfaces, bad for fine pitch. ENIG deposits 3 to 6 micrometres of nickel and 0.05 to 0.1 of gold on top: the gold is not luxury, it is a barrier that stops the nickel from oxidising, and its flatness is what lets you solder 0.3-millimetre balls on a BGA. OSP, an organic film removed by the first bath, and immersion silver also exist.

Not a single broken track

Before leaving the plant every panel goes through automated optical inspection, which compares the real pattern with the design, and an electrical test. The most flexible is the flying probe: two or three heads that land on each pad and check continuity and isolation, net by net, over thousands of points per board. Mass production uses a nail fixture, the bed of nails, touching everything at once. Impedance is also measured by time-domain reflectometry (TDR) on test coupons: 50 ohms on a single track, 90 or 100 on a differential pair, with a ten per cent tolerance.

And then the solder paste arrives

The bare board becomes a motherboard on the assembly line. A metal stencil 100 or 120 micrometres thick deposits solder paste on every pad; placement machines put components down at 50,000 to 100,000 per hour with about 30 micrometres of accuracy. Then the reflow oven: a four or five zone profile that climbs slowly to 150 or 180 degrees to activate the flux, spikes to 245 in the reflow zone and drops at 2 or 3 degrees per second. Get the profile wrong and you get cold joints that work today and fail in six months.

At the end, optical inspection again, X-ray for the BGAs, in-circuit test and JTAG boundary scan, which uses a chain of registers inside the chips themselves to check connections without nails. Then the metal shielding cans are glued down and the antenna area is left clear: copper and metal there would short-circuit the radio.

The whole journey explains something that usually surprises people: the board is one of the cheapest parts of a phone and, at the same time, the one that piles up the most process steps. You pay in water, energy and chemicals, not in materials. It also explains why a board is not designed in an afternoon: every microvia, every ground plane and every gap between tracks shapes impedance, noise and, in the end, whether the phone makes calls or does not.